| Product Name | Mild Steel Electrode | ||||||||
| Product No. | MHAE411-WE004 | ||||||||
| Standard | |||||||||
| GB | E4313 | ||||||||
| AWS | E6013 | ||||||||
| JIS | D4313 | ||||||||
| DIN | E4332 R3 | ||||||||
| Covering Type | High titania Potassium | ||||||||
| Welding Position | F,V,OH,H | ||||||||
| Chemical Composition | C | Mn | Si | S | P | Ni | Mo | Cr | V |
| Typical | 0.070 | 0.41 | 0.26 | 0.021 | 0.023 | 0.018 | 0.002 | 0.027 | 0.01 |
| Mechanical Properties of Deposited Metal | |||||||||
| Test Item | Tensile Strengh Rm (MPa) | Yield Point ReL (MPa) | Elongation A4 (%) | Akv1(J) | |||||
| Guarantee | 400-560 | 306 | 22 | 47 | |||||
| Reference Current(AC/DC) | |||||||||
| Electrode Diameter(mm) | Electrode Length(mm) | Welding Current(A) | |||||||
| 2.5 | 300 | 40-70 | 40-70 | 40-70 | |||||
| 3.2 | 350 | 70-110 | 70-110 | 70-110 | |||||
| 4.0 | 400 | 100-150 | 100-150 | 100-150 | |||||
| 5.0 | 400 | 200-260 | 200-260 | 200-260 | |||||
| Instructions | |||||||||
| Usually it does not need to be baked before use.If allowed to become damp the electrodes should be re-dried for 30~60 minutes at 150°C before use. | |||||||||
| Application | |||||||||
| Welding mild steel with normal tensile strength particularly suitable for intermittent welding to sheet and small workpoces. | |||||||||