| Product Name | High Tensile Strength Steel Electrode | ||||||||
| Product No. | MHAE411-WE017 | ||||||||
| Standard | |||||||||
| GB | E5018-1 | ||||||||
| AWS | E7018-1 | ||||||||
| DIN | E5154B10 | ||||||||
| Type of Covering | Low hydrogen Potassium Iron powder | ||||||||
| Welding Position | F,V,OH,H | ||||||||
| Chemical Composition | C | Mn | Si | S | P | Ni | Mo | Cr | V |
| Guarantee | 0.12 | 1.6 | 0.75 | 0.035 | 0.04 | 0.3 | 0.3 | 0.2 | 0.08 |
| Mechanical Properties of Deposited Metal | |||||||||
| Test Item | Tensile Strengh Rm (MPa) | Yield Point ReL (MPa) | Elongation A4 (%) | Akv1(J) | |||||
| Guarantee | ≥490 | ≥400 | ≥22 | ≥27(-30 ) | |||||
| Reference Current (AC≥70V or DC+) | |||||||||
| Electrode Diameter(mm) | Electrode Length(mm) | Welding Current(A) | |||||||
| 2.5 | 300 | 60-100 | 60-100 | 60-100 | |||||
| 3.2 | 350 | 80-140 | 80-140 | 80-140 | |||||
| 4.0 | 400 | 110-210 | 110-210 | 110-210 | |||||
| 5.0 | 400 | 160-230 | 160-230 | 160-230 | |||||
| Instructions | |||||||||
| 1.The Electrodes must be baked under 300~350 for an hour before Welding and used as soon as baking is completed. | |||||||||
| 2.The stains on the weldments,such as rust,oil stains,moisture,etc.,must be cleared away before Welding. | |||||||||
| 3.When Welding,short arc must be used and stringer bead is suitable. | |||||||||
| Application | |||||||||
| Used for Welding carbon steel and low-alloy steel structures,such as boilers,pressure vessels,pipelines etc. | |||||||||