| Product Name | Corrosion Resisting Low Alloy Steel Electrode | |||||||||
| Product No. | MHAE411-WE026 | |||||||||
| Standard | ||||||||||
| GB | E6015-D1 | |||||||||
| AWS | E9015-G | |||||||||
| JIS | D5816 | |||||||||
| DIN | DY5554BXXH5 | |||||||||
| Type of Covering | Low hydrogen Sodium | |||||||||
| Welding Position | F,V,OH,H | |||||||||
| Chemical Composition | C | Mn | Si | S | P | Cr | Ni | Mo | V | Cu |
| Guarantee | 0.023 | 1.27 | 0.45 | 0.016 | 0.019 | 0.52 | 0.69 | 0.24 | 0.14 | 0.3 |
| Mechanical Properties of Deposited Metal | ||||||||||
| Test Item | Tensile Strengh Rm (MPa) | Yield Point ReL (MPa) | Elongation A4 (%) | Akv1(J) | ||||||
| Guarantee | 645 | 560 | 22 | -40℃ 80 | ||||||
| Reference Current (DC) | ||||||||||
| Electrode Diameter(mm) | 2.0 | 2.5 | 3.2 | 4.0 | 5.0 | 5.8 | ||||
| Welding Current(A) | 60-80 | 70-90 | 90-120 | 140-180 | 170-210 | 210-260 | ||||
| Instructions | ||||||||||
| 1.The Electrodes must be baked under 300~350 for an hour before Welding and used as soon as baking is completed. | ||||||||||
| 2.The stains on the weldments,such as rust,oil stains,moisture,etc.,must be cleared away before Welding. | ||||||||||
| 3.When Welding,short arc must be used and stringer bead is suitable. | ||||||||||
| Application | ||||||||||
| Suitable for welding important structures made by atmospheric corrosion and marine water corrosion low alloy steels,e.g. WNQ570. | ||||||||||