| Product Name | Low Alloy Steel Electrode | |||||||||
| Product No. | MHAE411-WE035 | |||||||||
| Standard | ||||||||||
| GB | E7517-G | |||||||||
| AWS | E11015-G | |||||||||
| JIS | D7016 | |||||||||
| DIN | EY6924BXXH15 | |||||||||
| Type of Covering | low hydrogen sodium | |||||||||
| Welding Position | F,V,OH,H | |||||||||
| Chemical Composition of Deposited Metal (%) | ||||||||||
| Chemical Composition | C | Mn | Si | S | P | Cr | Ni | Mo | V | Cu |
| Guarantee | 0.070 | 1.85 | 0.40 | 0.012 | 0.016 | 0.006 | 0.010 | 0.50 | 0.07 | 0.015 |
| Mechanical Properties of Deposited Metal | ||||||||||
| Test Item | Tensile Strengh Rm (MPa) | Yield Point ReL (MPa) | Elongation A4 (%) | Akv1(J) | ||||||
| Guarantee | 780 | 680 | 18 | 100 | ||||||
| Reference Current (DC) | ||||||||||
| Electrode Diameter(mm) | 2.0 | 2.5 | 3.2 | 4.0 | 5.0 | |||||
| Welding Current(A) | 40-70 | 60-90 | 80-110 | 130-170 | 160-200 | |||||
| Instructions | ||||||||||
| 1.The Electrodes must be baked under 300~350 for an hour before Welding and used as soon as baking is completed. | ||||||||||
| 2.The stains on the weldments,such as rust,oil stains,moisture,etc.,must be cleared away before Welding. | ||||||||||
| 3.When Welding,short arc must be used and stringer bead is suitable. | ||||||||||
| Application | ||||||||||
| For welding important structures fabricated by 740MPa tensile strength or more low alloy steels. | ||||||||||