| Product Name | Stainless Steel Electrode | |||||||||
| Product No. | MHAE411-WE047 | |||||||||
| Standard | ||||||||||
| GB | E308-15 | |||||||||
| AWS | E308-15 | |||||||||
| DIN | E199B26 | |||||||||
| Type of Covering | Low hydrogen sodium | |||||||||
| Welding Position | F,V,OH,H | |||||||||
| Chemical Composition | C | Mn | Si | S | P | Cr | Ni | Mo | V | Cu |
| Guarantee | 0.060 | 1.30 | 0.47 | 0.007 | 0.024 | 19.88 | 9.90 | 0.13 | 0.18 | — |
| Mechanical Properties of Deposited Metal | ||||||||||
| Test Item | Tensile Strengh Rm (MPa) | Yield Point ReL (MPa) |
Elongation A4 (%) |
Akv1 (J) |
||||||
| Guarantee | 600 | 44 | ||||||||
| Reference Current (DC) | ||||||||||
| Electrode Diameter(mm) | 2.0 | 2.5 | 3.2 | 4.0 | 5.0 | |||||
| Length(mm) | 300 | 300 | 350 | 400 | 400 | |||||
| Welding Current(A) | 25-50 | 50-80 | 80-110 | 110-160 | 160-180 | |||||
| Instructions | ||||||||||
| 1.The Electrodes must be baked under 250℃ for an hour before Welding. | ||||||||||
| 2.The stains on the weldments,such as rust,oil stains,moisture,etc.,must be cleared away before Welding. | ||||||||||
| Application | ||||||||||
| For welding corrosion resisting structures made by 06Cr18Ni9 stainless steel,which working temperature is lower than 300℃. It could welding high Cr steels or surfacing also. | ||||||||||