| Product Name | Stainless Steel Electrode | |||||||||
| Product No. | MHAE411-WE049 | |||||||||
| Standard | ||||||||||
| GB | E308L-16 | |||||||||
| AWS | E308L-16 | |||||||||
| JIS | D308L | |||||||||
| DIN | E199ncR23 | |||||||||
| Type of Covering | Extra low carbon Lime titania | |||||||||
| Welding Position | F,V,OH,H | |||||||||
| Chemical Composition | C | Mn | Si | S | P | Cr | Ni | Mo | V | Cu |
| Typical | 0.030 | 1.28 | 0.72 | 0.012 | 0.022 | 19.50 | 9.70 | 0.03 | 0.10 | — |
| Mechanical Properties of Deposited Metal | ||||||||||
| Test Item | Tensile Strengh Rm (MPa) | Elongation A4 (%) | ||||||||
| Typical | 650 | 35 | ||||||||
| Reference Current (AC or DC) | ||||||||||
| Electrode Diameter(mm) | 2.0 | 2.5 | 3.2 | 4.0 | 5.0 | |||||
| Length(mm) | 300 | 300 | 350 | 400 | 400 | |||||
| Instructions | ||||||||||
| 1.The Electrodes must be baked under 250℃ for an hour before Welding. | ||||||||||
| 2.The weldment must be preheated to 250-350℃ before Welding. | ||||||||||
| Application | ||||||||||
| Especially for surfacing the inner chamber of hydrocracking reactor. | ||||||||||