Product Name | Stainless Steel Electrode | |||||||||
Product No. | MMDE411-WE063 | |||||||||
Standard | ||||||||||
GB | AWS | JIS | DIN | |||||||
E410-15 | E410-15 | E13B20+ | ||||||||
Type of Covering | Low hydrogensodium | |||||||||
Welding Position | F,V, OH,H | |||||||||
Chemical Composition of Deposited Metal (%) | ||||||||||
Chemical Composition | C | Mn | Si | S | P | Cr | Ni | Mo | V | Cu |
Standard | ≤0.12 | ≤1.00 | ≤0.90 | ≤0.030 | ≤0.040 | 11.0-13.5 | ≤0.70 | ≤0.75 | ≤0.75 | — |
Typical | 0.061 | 0.57 | 0.48 | 0.007 | 0.023 | 12.26 | 0.31 | 0.011 | 0.031 | — |
Mechanical Properties of Deposited Metal | ||||||||||
Test Item | Tensile Strengh Rm (MPa) | Elongation A4 (%) | ||||||||
Standard | ≥450 | ≥20 | ||||||||
Typical | 545 | 29 | ||||||||
Reference Current (DC) | ||||||||||
Electrode Diameter(mm) | 3.2 | 4.0 | 5.0 | |||||||
Welding Current(A) | 80-120 | 100-160 | 150-200 | |||||||
Instructions |
||||||||||
1.The Electrodes must be baked under 250℃ for an hour before Welding. |
||||||||||
2.The weldment must be preheated to 250-350℃ before Welding. |
||||||||||
Application |
||||||||||
It is suitable for welding structures made by 06Cr13 or 1Cr13 stainless steels, also can be used for surfacing corrosion resisting and abrasion. |