| Product Name | Nickel or Nickel Based Alloy Electrode | ||||||||||
| Product No. | MHAE411-WE075 | ||||||||||
| Standard | |||||||||||
| GB | ENiCrFe-3 | ||||||||||
| AWS | ENiCrFe-3 | ||||||||||
| JIS | DNiCrFe-3 | ||||||||||
| Type of electrode | Low hydrogen | ||||||||||
| Welding Position | F,V,OH,H | ||||||||||
| Chemical Composition | C | Mn | Fe | P | S | Si | Cu | Ni | Cr | Nb+Ta | other |
| Guarantee | ≤0.10 | ≤5.0-9.5 | ≤10.0 | ≤0.03 | ≤0.015 | ≤1.0 | ≤0.50 | ≥59 | 13.0-17.0 | 1.0-2.5 | ≤0.50 |
| Mechanical Properties of Deposited Metal | |||||||||||
| Test Item | Tensile Strengh Rm (MPa) | Elongation A4 (%) | |||||||||
| Guarantee | ≥550 | ≥30 | |||||||||
| Reference Current (AC or DC) | |||||||||||
| Electrode Diameter(mm) | 2.5 | 3.2 | 4.0 | ||||||||
| Welding Current(A) | 40-70 | 80-100 | 110-150 | ||||||||
| Instructions | |||||||||||
| 1.The Electrodes must be baked under 300~350 for an hour before Welding and used as soon as baking is completed. | |||||||||||
| 2.The stains on the weldments,such as rust,oil stains,moisture,etc.,must be cleared away before Welding. | |||||||||||
| Application | |||||||||||
| Suitable for welding structures made by UNS N06600 NiCrFe alloy,composite NiCrFe alloy and dissimilar metals of nickel alloy with steel. Also surfacing. | |||||||||||